dc.description.abstractEl objetivo del presente estudio de investigación es determinar la variación de las propiedades físico- mecánicas con la adición de cal (2 y 4%) y cemento (7; 9 y 11%) respectivamente, en suelos arcillosos procedentes de la vía Agua Buena- Colegio La Salle que serán utilizados para subrasante. El enfoque de investigación es de corte cuantitativo, el nivel o alcance corresponde al nivel descriptivo explicativo, y en cuanto a diseño es una investigación experimental. Se realizaron ensayos en laboratorio con adición de cal en peso en las proporciones de 2 y 4% y con cemento de 7; 9 y 11% respectivamente, luego se presentan los resultados del análisis de las propiedades del suelo con adición de cal y cemento en las proporciones señaladas se presenta en tablas y figuras, a partir de estas se establecen las variaciones en las características físico-mecánicas para el empleo en subrasante. A partir del análisis e interpretación de los resultados se concluye que los valores del índice de plasticidad con adición de cal oscilan entre el 7.34 y el 7.77%; mientras que con adición de cemento fluctúan entre 4.55 y 5.05%, observándose, con aditamento de cemento existe una disminución de índice de plasticidad; las pruebas de compactación utilizando energía modificada con cal y cemento como aditivos, el contenido de humedad óptimo con la adición de 9% de cemento es la más representativa al 11,95% a una densidad seca máxima de 1,69gr/cm ; el índice de CBR al 95% densidad seca máxima se logra con adición de cemento a una proporción de 11% obteniéndose un porcentaje de 10,50%, y las pruebas de resistencia a la compresión inconfinada se puede señalar que el esfuerzo o resistencia del suelo se logró una mejor cohesión con adición de cemento al 11%. 3es_PE
dc.description.abstractThe objective of this research study is to determine the variation of the physical-mechanical properties with the addition of lime (2 and 4%) and cement (7; 9 and 11%) respectively, in clay soils from the Agua Buena-Colegio La Salle road that will be used for subgrade. The research approach is quantitative, the level or scope corresponds to the explanatory descriptive level, and in terms of design it is an experimental research. Laboratory tests were carried out with the addition of lime by weight in the proportions of 2 and 4% and with cement of 7; 9 and 11% respectively, then the results of the analysis of the properties of the soil with the addition of lime and cement in the proportions indicated are presented in tables and figures, from these the variations in the physical-mechanical characteristics for the use in subgrade are established. From the analysis and interpretation of the results it is concluded that the values of the plasticity index with lime addition range between 7.34 and 7.77%; while with the addition of cement they fluctuate between 4.55 and 5.05%, observing, with cement attachment there is a decrease in the plasticity index; compaction tests using energy modified with lime and cement as additives, the optimal moisture content with the addition of 9% cement is the most representative at 11.95% at a maximum dry density of 1.69gr/cm3; the CBR index at 95% maximum dry density is achieved with the addition of cement at a proportion of 11% obtaining a percentage of 10.50%, and the tests of resistance to unconfined compression can be indicated that the stress or resistance of the soil was achieved a better cohesion with the addition of cement at 11%.en_US
dc.formatapplication/pdfes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Andina del Cuscoes_PE
dc.rightsinfo:eu-repo/semantics/openAccesses_PE
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/es_PE
dc.subjectPropiedades fisco mecánicases_PE
dc.subjectEstabilización del sueloes_PE
dc.subjectAdición de cal y cementoes_PE
dc.titleAnálisis comparativo de las características físico-mecánicas de suelos arcillosos en la vía Agua Buena- Colegio La Salle con la adición de cal (2 y 4%), y cemento (7; 9 y 11%) para subrasantees_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.nameIngeniero Civiles_PE
thesis.degree.grantorUniversidad Andina del Cusco. Facultad de Ingeniería y Arquitecturaes_PE
thesis.degree.disciplineIngeniería Civiles_PE
dc.publisher.countryPEes_PE
dc.subject.ocdehttps://purl.org/pe-repo/ocde/ford#2.01.01es_PE
renati.advisor.dni23928061
renati.advisor.orcidhttps://orcid.org/0000-0003-2401-707Xes_PE
renati.author.dni72437918
renati.discipline732016es_PE
renati.jurorCalderón Gonzales, Werner Alfonso
renati.jurorChipana Molina, Yimmy Johan
renati.jurorVera Gallegos, Ronald
renati.jurorPeñalva Gallegos, Zandro
renati.levelhttps://purl.org/pe-repo/renati/level#tituloProfesionales_PE
renati.typehttps://purl.org/pe-repo/renati/type#tesises_PE


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record

info:eu-repo/semantics/openAccess
Except where otherwise noted, this item's license is described as info:eu-repo/semantics/openAccess